dc.contributor.authorRiosalido, Paula M.-
dc.contributor.authorVelásquez, Pablo-
dc.contributor.authorMurciano Cases, Ángel-
dc.contributor.authorDe Aza, Piedad-
dc.contributor.otherDepartamentos de la UMH::Ciencia de Materiales, Óptica y Tecnología Electrónicaes_ES
dc.date.accessioned2025-02-25T08:22:30Z-
dc.date.available2025-02-25T08:22:30Z-
dc.date.created2025-
dc.identifier.citationCeramics Internationales_ES
dc.identifier.issn1873-3956-
dc.identifier.issn0272-8842-
dc.identifier.urihttps://hdl.handle.net/11000/35721-
dc.description.abstractIn this investigation, three distinct multiphasic scaffolds, comprising primary crystalline phases of SiO₂, Ca₂P₂O₇, and Ca₃(PO₄)₂, were developed. These scaffolds feature surface coatings that have been functionalised with Na, K, and varying molar proportions of Mg (0–1%). The samples were extensively characterised to evaluate a number of key properties including microstructure, porosity, mechanical properties, biodegradation profile, biocompatibility and in vitro bioactivity. The scaffolds demonstrated a mechanical strength of 1.8 MPa, accompanied by a high macroporosity of over 85 % and micropores ranging from 200 to 6 μm. All scaffolds showed bioactivity. Notably, CS0.7 Mg exhibited a distinctive topography characterised by non-periodic, irregular lamellae at both the micro- and nanoscale. During the bioactivity assays, the lamellae were progressively covered by HA until they were completely obscured after 14 days in SBF. This bioactive behaviour was accompanied by gradual degradation in PBS, with a 15 % weight loss over 21 days, indicating suitability for bone regeneration. In addition, ICP-OES analysis demonstrated ionic exchange from the scaffolds into the culture medium at both concentrations of 15 mg/mL and 30 mg/mL, which promoted the proliferation of 3T3 fibroblasts. Cells seeded on the CS0.7 Mg scaffold also showed sustained cell proliferation over time. This proliferation was found to be influenced by the topography of the scaffold, with the greatest enhancement observed in the CS0.7 Mg-7D samples, which had HA-covered lamellae.es_ES
dc.formatapplication/pdfes_ES
dc.format.extent11es_ES
dc.language.isoenges_ES
dc.publisherElsevieres_ES
dc.relation.ispartofseries51es_ES
dc.rightsinfo:eu-repo/semantics/openAccesses_ES
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/4.0/*
dc.subjectSol-gel processeses_ES
dc.subjectPorosityes_ES
dc.subjectGlass ceramicses_ES
dc.subjectBiomedical applicationses_ES
dc.subject.otherCDU::6 - Ciencias aplicadas::62 - Ingeniería. Tecnologíaes_ES
dc.titleMultilayer scaffolds designed with bioinspired topography for bone regenerationes_ES
dc.typeinfo:eu-repo/semantics/articlees_ES
dc.relation.publisherversionhttps://doi.org/10.1016/j.ceramint.2025.01.180es_ES
Appears in Collections:
Artículos - Ciencia de los materiales, óptica y tecnología electrónica


Thumbnail

View/Open:
 1-s2.0-S027288422500207X-main.pdf
6,3 MB
Adobe PDF
Share:


Creative Commons ???jsp.display-item.text9???